It is 11 "H,15"W, and 1 1/2 D. A pate de verre high relief type piece of a boy throwing a ball into ocean with two dalmation dogs jumping up in the surf. The devit(molted irregular white scum) appears randomly all over the marine blue ocean and sky bue sky, but the boy and dogs are fine. thought I would mask the figures and dogs, sand blast, then seal with Watco Danish oil.
How can I mask off the figures and dogs?I heard elmer's glue could be used, but then how do I remove it cleanly without disturbing the background which will be sandblasted. I hate the blasted devit. I think I held it too long at melting point.
Any suggestions? Is there a better sealer than the Watco oil?
Thanks,