Page 1 of 1

First Combing Try

Posted: Tue Mar 09, 2004 11:56 pm
by joeat
My first attempt at combing, i probably didn't move tool around enough,
but as i said it's my first attempt. Let me know what you think. The help
that i get here makes me want to try new things, and i know that i will
only get good advice.
Thanks
John
http://community.webshots.com/photo/124 ... 0656XtDzuZ

Posted: Wed Mar 10, 2004 12:28 am
by Nutty,Dave
i like it !!!

i have not done any combing yet (need some heat protection first) ... what temp did you take it to ???

Posted: Wed Mar 10, 2004 12:48 am
by joeat
I took it to 1700, then i combed, then held at 1700 for 30 min. I was a
little afraid that i would comb too hard and go thru glass into shelf.