I've been making some drop ring vases recently and thought it'd be easy to get some iron and bend it into a simple holder.  I've discovered that metal is much more uncooperative than I anticipated and would like to know if anyone could guide me to some info on how to do it. I've tried 1/8" iron and 1/4" braising rod, heating them with a propane torch then bending them around an old piece of 2" pipe. The bends always turn out really funky instead of nice smooth round curves I envision. Any assistance would be greatly appreciated!
Pam
			
			
									
						
										
						Pam
- 
				Tyler Frisby
 - Posts: 75
 - Joined: Tue Dec 02, 2003 8:27 pm
 - Location: Canada
 
Try an Oxygen + acetalyne torvh, it burns hotter and gives a more needle pointed style flame tip alloing for more controlled (precise)heating, thus giving the ability to get 90 deg angles and stuff. I played with one for a while and I want one, there too kool. 
you can rent the tanks by the month a nd just pay for gas , but i think you'll be stuck buying the torch part
Hope I helped,
Tyler
			
			
									
						
										
						you can rent the tanks by the month a nd just pay for gas , but i think you'll be stuck buying the torch part
Hope I helped,
Tyler
- 
				Bert Weiss
 - Posts: 2339
 - Joined: Tue Mar 11, 2003 12:06 am
 - Location: Chatham NH
 - Contact:
 
Re: bending metal rod for drop ring vase
Ask a blacksmith shop to make them.Pam wrote:I've been making some drop ring vases recently and thought it'd be easy to get some iron and bend it into a simple holder. I've discovered that metal is much more uncooperative than I anticipated and would like to know if anyone could guide me to some info on how to do it. I've tried 1/8" iron and 1/4" braising rod, heating them with a propane torch then bending them around an old piece of 2" pipe. The bends always turn out really funky instead of nice smooth round curves I envision. Any assistance would be greatly appreciated!
Pam
Bert 
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
			
						Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
- 
				Clifford Ross
 - Posts: 68
 - Joined: Sun Mar 09, 2003 10:08 pm
 - Location: Myrtle Beach, So. Carolina
 - Contact:
 
- 
				Dick Kolpack
 - Posts: 17
 - Joined: Tue Mar 18, 2003 4:47 pm
 - Location: Arizona
 - Contact:
 
- 
				Tony Serviente
 - Posts: 328
 - Joined: Thu May 29, 2003 11:48 am
 - Location: Ithaca,NY
 - Contact:
 
$49.99 ring forming machine.
I prefer using inexpensive benders for truely smoothe curves. Http://www.harborfreight.com has a couple of products that will bend or make rings. Item #36790-0VGA Planetary Ring Roller will make rings from 3" to several feet in diameter. This tool is $49.99 and is suitable for modest use. They also have a general purpose bender that sells for about $79.00.