Page 1 of 1
					
				Bas relief slump
				Posted: Fri Apr 09, 2004 2:05 pm
				by M.L.
				Couldn't find in the archive, so here's the question.  Float glass circle 10in., 1/4in. glass.  Using fiber paper design cut out.  When slumping into a SS bowl, will I lose much of the design element.  Thanks  Mike
			 
			
					
				Re: Bas relief slump
				Posted: Fri Apr 09, 2004 2:29 pm
				by Brock
				Mike Boos wrote:Couldn't find in the archive, so here's the question.  Float glass circle 10in., 1/4in. glass.  Using fiber paper design cut out.  When slumping into a SS bowl, will I lose much of the design element.  Thanks  Mike
Shouldn't lose any Mike, slump low and slow.  Brock
 
			
					
				
				Posted: Fri Apr 09, 2004 2:36 pm
				by M.L.
				Thanks Brock.  Have a good weekend.  Mike
			 
			
					
				
				Posted: Fri Apr 09, 2004 2:38 pm
				by Brock
				U2 Mike. Bono