				How fast to fire a pot melt
				Posted: Sat Apr 10, 2004 8:48 pm
				by Lonman
				Can anybody please tell me how fast to get up to 1600+ degrees for a pot melt?  Or does it even matter?
Thanks
Lonman 

 
			
					
				
				Posted: Sat Apr 10, 2004 9:51 pm
				by Steve Immerman
				It only matters that if you go too fast it is theoretically possible that your pot or your shelf could crack. I usually use 2000dph.
Steve
			 
			
					
				Pot melt
				Posted: Sun Apr 11, 2004 2:19 pm
				by revjerry
				Steve,
I'd like to see your kiln!  Are you really able to make 1600 in less than an hour?  Hate to have your electric bill.  But that's a good answer.  I know that my kiln doesn't go much faster than 900 an hour but I don't like going that fast.  You know my process, and within that process I usually go at 600 an hour to protect the pots, kiln and the base glass.  Probably faster won't hurt anything.
BTW, a customer was in the shop this week and asked if I'd ever considered making a pot melt into a table top?  Interesting thought.  Certainly there's size limits, but I think it can be done.  Anyway, there's some new food for thought.
Will I see you in Corning?
Jerry
			 
			
					
				Re: Pot melt
				Posted: Sun Apr 11, 2004 5:05 pm
				by Steve Immerman
				Revjerry wrote:Steve,
I'd like to see your kiln!  Are you really able to make 1600 in less than an hour?  Hate to have your electric bill.  But that's a good answer.  I know that my kiln doesn't go much faster than 900 an hour but I don't like going that fast.  You know my process, and within that process I usually go at 600 an hour to protect the pots, kiln and the base glass.  Probably faster won't hurt anything.
Will I see you in Corning?
Jerry
I have a Paragon GL22 with elements in the top, side and doors. I don't exactly know how fast it heats up when I set it to 2000dph. Never timed it. Next time, I'll keep an eye on the clock.
Not sure about Corning yet.
Steve
 
			
					
				
				Posted: Sun Apr 11, 2004 5:10 pm
				by Brock
				I'd like to see your kiln! Are you really able to make 1600 in less than an hour?
There's a certain engineer type on this board who has built the fastest kiln I've ever heard of.
Brock
			 
			
					
				
				Posted: Tue Apr 13, 2004 8:33 pm
				by Phil Hoppes
				Hmm....now who would that be....
Can you say 3000 DPH!!
FireBoy
OBTW.....not the fastest.  A prof at my old Alma Mater did a little better
http://www.discoverchemistry.com/dcv2-d ... fault.html
He got to 10,000 degrees in about 1/2 second.  The faculty made him take down his web site.  

   I saw it before they made him remove it.  VERY IMPRESSIVE!!!!
 
			
					
				
				Posted: Thu Apr 15, 2004 5:19 pm
				by Havi
				 
 
can you excuse me? what is pot melting? do you use a wok for this?? sorry to be such ignorant....... perhaps this is something new I could enjoy??
thanks,
 
			
					
				
				Posted: Thu Apr 15, 2004 6:15 pm
				by Cynthia
				heruviva wrote: 
 
can you excuse me? what is pot melting? do you use a wok for this?? sorry to be such ignorant....... perhaps this is something new I could enjoy??
thanks,
 
Havi,
There's a great book called 
Techniques of Kiln-formed Glass by Keith Cummings.  In it he describes what he calls a 'kiln pour' and many variations on pouring... among many other techniques that we talk about on this board.  If you want to learn many many different way to form glass in a kiln, this is THE book.  Lots of information, history, great pictures...and more techniques than you can possibly ever even try.
A pot melt is simply a variant of pouring...Fill a clay flower pot with three colors of glass, divided into three sections, suspend the pot above the shelf with a bridge of kiln furniture and heat to about 1700F until it starts to flow out of the drainage hole and onto the shelf giving you a spiral design of how the glass flows onto the shelf (think honey off of a spoon...spin, drizzle).
 
			
					
				
				Posted: Fri Apr 16, 2004 12:27 am
				by Havi
				Thank you guys for the pm's and the on board explanations!
 I am very grateful! I remember now I tried this in one of the workshops I attended, it was not very successful, though 
hopefully I shall try it again 
 
  