Page 1 of 1
Fused Panels for my back splash
Posted: Tue Apr 13, 2004 7:47 am
by Michael McNerney
Hello everyone.
I just wanted to share my current project with you all and get your feed back.
http://groups.msn.com/McNerneyGlassAlbu ... PhotoID=13
Thanks
Michael
Being hung
Posted: Tue Apr 13, 2004 7:48 am
by Michael McNerney
Posted: Tue Apr 13, 2004 11:03 am
by Phil Hoppes
Very cool. Simple but elegant. How were they made? Looks like mica's on black glass with some red fused for the berries.
Phil
Posted: Tue Apr 13, 2004 11:26 am
by Michael McNerney
Phil,
Good Guess.
They are Black Bullseye with mica applications and Dichro Beads.
Michael
Posted: Tue Apr 13, 2004 11:50 am
by Nancy Juhasz
Mike,
Very nice. I am starting to see a pattern in your work. When I saw the picture of the tiles my thoughts were that is definately Mike's work. If you get boared well you know the line...........................
Nanc
Posted: Wed Apr 14, 2004 6:16 am
by rhonday
those are gorgeouse micheal such great detail work
Rhonda
Posted: Wed Apr 14, 2004 12:09 pm
by Kathie Karancz

Awesome Michael
very cool

McNearney pics
Posted: Thu Apr 15, 2004 1:21 pm
by bernie
Michael, I can't download your pics. I get some msn garbage wanting
to do a birthday thing and a chat. I hate that. Looks like others have
been able to click and it opens. Any suggestions? Bernie