Page 1 of 1
					
				plaster water ratio
				Posted: Fri Apr 16, 2004 8:24 pm
				by Liam
				I moved. Ive lost my firing log.  My life may be over.
anyways, now I need a recipe for plater water for 1500 deg casting.  I need a volume one not weight.  Does anyone have one?  thanks if you can help.
Liam
			 
			
					
				Re: plaster water ratio
				Posted: Fri Apr 16, 2004 11:11 pm
				by Bert Weiss
				Liam wrote:I moved. Ive lost my firing log.  My life may be over.
anyways, now I need a recipe for plater water for 1500 deg casting.  I need a volume one not weight.  Does anyone have one?  thanks if you can help.
Liam
As much plaster mix as you can get in the water and still manage to get a pour with some resolution.  The less plaster to water, the easier it is to pour and the weaker the mold.  More plaster, stronger mold.
 
			
					
				
				Posted: Sun Apr 18, 2004 8:15 pm
				by charlie holden
				Mixes based on volume are not accurate since a given volume of dry powder may be firmly packed or lightly packed.  If you don't have a scale just pour the dry mix into the water untill it peaks, let it slake for 5 minutes then mix.
ch