wire for wine bottle fuse
Posted: Mon Apr 19, 2004 10:08 am
Just a quick question regarding the hangers for slumped wine bottles, how is it possible to attach a wire to hang the finished product, I've tried glue, doesn't hold,
even fusing a piece of wire into the glass, but it cracks, any suggestions? thanks