Page 1 of 1
Firesticks
Posted: Sun Apr 13, 2003 10:19 pm
by Vickie
I'm making kiln formed bracelets, and saw a cool thing called "Firesticks" to tack fuse on the fused glass. Paclific Art Glass is the only place I could find that sells them..problem is that they only sell wholesale, and a 250.00 minimum. Has anyone worked with these before, or know where else I could buy them retail? Sorry for the above misspelling, it's Pacific Art Glass. Any help would be appreciated
Vickie
Posted: Mon Apr 14, 2003 1:08 am
by Cristi
You don't need a resale number to shop at Pacific Art Glass and the minimum purchase is $50, although it's very easy to spend more.-Cristi
Posted: Mon Apr 14, 2003 8:28 pm
by Linda Hassur
What is a firestick? Linda
Posted: Wed Apr 16, 2003 2:49 pm
by K Okahashi
Vicki,
You can also order them directly from Phil and Hazel Teefy at
http://www.glassglow.com. They are in Sacramento California and Hazel can help you with that.
I also know that Bonita Sherman at Artistic Glass Specialties sells them too. They are located in Las Vegas. 702-876-4527 (Don't know if they send thru the mail though).
I believe Pacific Art goes to many many shows too and brings these with them. They are wavey dichroic strips...very cool but they run out quickly. Good luck.