Page 1 of 1

French cleats, source for

Posted: Tue Apr 15, 2003 9:01 pm
by Paul Housberg
Back on the old board someone had posted a source for aluminum (I think) French cleats. Found the thread but couldn't find the source (link may be dead). Can anyone help?

Thanks,
Paul

Posted: Tue Apr 15, 2003 9:49 pm
by Ron Coleman

Posted: Tue Apr 15, 2003 10:11 pm
by Barbara Muth
If you are interested in acrylic French cleats, I am working with a fabricator and should be able to distribute some shortly. They work well with translucent pieces.

Will post on classifieds once I have some questions resolved.

Barbara

Posted: Tue Apr 15, 2003 11:32 pm
by Mike Byers
There are also some steel cleats that work the same way; they're called "Z-bar" and can be ordered from most framing shops.

Posted: Wed Apr 16, 2003 10:15 am
by charlie
1/2" plywood. 4" wide piece ripped at 45 degree angle down the middle.