Page 1 of 1
Stereo Pot melt
Posted: Wed Apr 30, 2003 10:50 am
by Jerry
Here's a little something I did in my last crazed state of mind; kind of looks like that too. Now, if I can figure out how to post the picture.

Posted: Wed Apr 30, 2003 11:32 am
by Helen O'Neill
How marvelous!

What colors did you use for this melt?
stereo Pot Melt
Posted: Wed Apr 30, 2003 1:11 pm
by Jerry
Spectrum series 96, black, white and orange. Looks kinda like halloween.
Jerry
Posted: Wed Apr 30, 2003 1:20 pm
by Jerry Cave
Jerry - I love the colors.
Can you tell me how you posted that photo in your post?
thanks
the other jerry
Posted: Wed Apr 30, 2003 1:40 pm
by Randy W
Jerry, that is way cool !

I've wanted to try multiple pots but just don't have the time right now. It's beautiful! Thanks for sharing.
Randy
Pot melt photo
Posted: Wed Apr 30, 2003 2:56 pm
by Jerry
Jerry,
If you check the part of the board called "board help" there's plenty of information on how to do it. Basically you have to have your picture on a web site somewhere. I put mine on my ISPs personal web site; most ISPs do that. Then, in the post, when I got to the point that I wanted the picture, I clicked on "Img" in the icons above, put in the link and clicked "Img" again. It works really slick.
Glad you liked the work too.
Jerry
Posted: Wed Apr 30, 2003 3:13 pm
by Jerry Cave
Jerry,
Thanks for the tip. I kept missing the "img" part.
jerry
Posted: Wed Apr 30, 2003 3:16 pm
by Steve Immerman
Jerry,
Beautiful melt! Did you add the rim later, or place it under the melt?
Steve
Posted: Wed Apr 30, 2003 4:52 pm
by Suzan
Jerry, when you stacked the glass, did you put the same colour of glass all together or did you stack the different colours randomly?
Posted: Wed Apr 30, 2003 8:08 pm
by Clifford Ross
Stunning !!!
Posted: Thu May 01, 2003 10:18 am
by dinah ihle
That is a beautiful piece.
Posted: Sun May 04, 2003 8:53 am
by Phil Brown
Beautiful!!!
But how do you do the rim?
Thanks for the tip on posting.