Page 1 of 1
Happy Accident!
Posted: Sat May 03, 2003 1:25 am
by Aryana B. Londir
Here's an example of a happy accident! The mold broke during the slumping (don't know why!) but the result is quite cool......any comments?
http://aryana2.com/images/red_w_patern_ ... n_end2.jpg
Accident
Posted: Sat May 03, 2003 11:37 am
by Jerry
That's a nice piece. Sometimes those accidents are great and the piece tells us what it wants to be. Without seeing your mold I can only guess why that happened, but it looks like the mold may have been thin in that area and gave way under the weight of the glass. That's just a guess.
Anyway, congrats, it's still a neat piece
Jerry
happy accident
Posted: Mon May 05, 2003 10:57 pm
by Aryana B. Londir
thanks for your compliment!
aryana
Posted: Tue May 06, 2003 9:57 am
by Zane
Very nice piece! I like it very much.
What are its dimensions?
Zane
happy accident
Posted: Tue May 06, 2003 11:10 am
by Aryana B. Londir
hi, it's 11" diameter.......and thanks! it really was one of those cool kiln surprises....funny how every piece since then has been fusing and slumping perfectly since that sacrifice to the kiln god!
![Smile :)](./images/smilies/icon_smile.gif)