Page 1 of 1

can you fix bubbles after fusing?

Posted: Sun May 04, 2003 2:46 pm
by Stacey Jones
I just fused a piece that took about 40 hours to make! Unfortunately I learned that bubbles form when the two layers of glass are not touching. I used frit on the lower peace of glass, and the bubbles formed inbetween the areas of the frit (big bubbles). Is there anyway to rescue this piece?
For instance, can I drilll a small hole in the bubbled area and then refire?
Thanks, Stacey

Posted: Sun May 04, 2003 5:04 pm
by Steve Immerman
There are many posts in the archives about this that you might find helpful.

I have tried drilling out the holes, and filling them with an appropriate color frit with good results.

Steve