This may have been mentioned already, but I missed it, if so.... have any of you tried putting a potmelt through a drop mold? Is it cool or uuug-ly?
Thanks.... I want to learn from your mess... er, experience before I try this.
I'm waiting too Dani, I've tried a few pot melts but haven't tried dropping it. I'll be interested to see what anyone has tried. I may get up enough nerve to try it myself.
Come on all you pot melters...SPEAK UP...
If I could free up my kilns for a pot melt I'd try it myself, too! But, I'm working like crazy to get a dozen bowls for a show and in the midst of moving.... yikes! Surely, somebody out there has a less-than-awesome pot melt they can try to drop through a mold? Yes?? Does it sound potentially cool to someone else out there?