Q: Pot Melt Masters

Posted: Mon May 12, 2003 2:14 pm
by Dani
This may have been mentioned already, but I missed it, if so.... have any of you tried putting a potmelt through a drop mold? Is it cool or uuug-ly?
Thanks.... I want to learn from your mess... er, experience before I try this. :wink:

Posted: Tue May 13, 2003 3:06 pm
by Dani
Okay, so was this just an incredibly STUpid question?? Or hasn't anyone tried it? I find it hard to believe the latter with this creative bunch.

Posted: Tue May 13, 2003 7:17 pm
by Diane
I'm waiting too Dani, I've tried a few pot melts but haven't tried dropping it. I'll be interested to see what anyone has tried. I may get up enough nerve to try it myself.
Come on all you pot melters...SPEAK UP...

Posted: Tue May 13, 2003 7:22 pm
by Dani
If I could free up my kilns for a pot melt I'd try it myself, too! But, I'm working like crazy to get a dozen bowls for a show and in the midst of moving.... yikes! Surely, somebody out there has a less-than-awesome pot melt they can try to drop through a mold? Yes?? Does it sound potentially cool to someone else out there?