Am I going to CRY????
Posted: Wed May 14, 2003 9:54 am
				
				I have been doing some 2x2 and 3x3 tiles with the kids at the school where I do technology.  We have a large programable skutt kiln. I have fired 3 batches.  The tiles have been turning our great.  
 
this is the schedule I have been using
600 1480 20
9999 970 20
120 850 0
200 700 0
off
Loaded the kiln yesterday at lunch. Turned it on, used the same program as before. Something went wrong. The kiln did not shut off. So the tiles have been at about 1300 since yesterday.
I was able to program it to heat just a little and then cool down using the same schedule at before.
AM I going to be crying and having kids cry when I open it?
What a way to start the morning.
KRIS
			this is the schedule I have been using
600 1480 20
9999 970 20
120 850 0
200 700 0
off
Loaded the kiln yesterday at lunch. Turned it on, used the same program as before. Something went wrong. The kiln did not shut off. So the tiles have been at about 1300 since yesterday.
I was able to program it to heat just a little and then cool down using the same schedule at before.
AM I going to be crying and having kids cry when I open it?
What a way to start the morning.