Page 1 of 1
Sandpiper did it...Yea!!!!
Posted: Wed May 14, 2003 11:43 am
by Sandpiper
I did it. I fused. I slumped. I got a bowl. No bubbles. Nice shiny surface. Yippeee. The design is not so great and the rim is a little smunched (technical term) But it is a bowl. Thanks so much for all your help. I'm so grateful. I'm going to try to attach a picture of the first born, but I may not do it right. Okay, I couldn't make the picture work. So darn much to learn. If anyone is bored and want to explain how to put a picture at the end of this message. I would appreciate it. Thanks
I gotta go melt something
Sandpiper
Posted: Wed May 14, 2003 12:06 pm
by Tony Smith
Congratulations... it really is exciting... you feel like you just gotta melt something... all the time.
As far as posting a photo, you need to be able to place it on the internet in either a website or one of the many free photo sites and post the link to the photo in your message. "[img]"%20goes%20before%20your%20photo%20and%20"[/img]" goes after.
Tony
Posted: Wed May 14, 2003 12:24 pm
by Sandpiper
I still can't make the picture attach, but if anyone wants to look I stuck it at the bottom of my pathetic little website. So go to my homepage and scroll to the bottom. Cheers.
Sandpiper
http://www.sandpipercottagestudios.com
Posted: Wed May 14, 2003 2:07 pm
by mybigsister
Sandpiper - Cool bowl! I have two of the whoops on the edge of my 1st bowl. Mine were caused by original break that I refused and then reslumped......Pat in WA
Posted: Wed May 14, 2003 3:11 pm
by Sandpiper
Thank you. At least the rim problem is right at the design. So, I call it an organic process as the pea pod grows. Or some other BS like that

(It wasn't supposed to look like a pea pod design, but my helpful family proclaimed that it was a pea pod, so okay, it's a pea pod.)
Sandpiper
Posted: Wed May 14, 2003 4:16 pm
by Tess Farley
Your bowl is beautiful! Isn't this fun!!!!
Posted: Wed May 14, 2003 4:16 pm
by Tess Farley
Your bowl is beautiful! Isn't this fun!!!!
Posted: Wed May 14, 2003 7:09 pm
by Kitty
i think your bowl is wonderful, especially for a first attempt!
Posted: Wed May 14, 2003 9:18 pm
by Tracy
Your bowl has beauty and spirit! Keep up your creative style!

-Tracy
Great Bowl!
Posted: Wed May 14, 2003 10:28 pm
by Terri Johanson
You are on your way now...you won't be able to stop!
Terri