Page 1 of 1
					
				ed hoy,,,FUSERS GLUE
				Posted: Mon May 19, 2003 2:37 pm
				by rodney
				I need to get a price on the ed hoy fusers glue, but they wont even give me a quote because i havent sent them my life story,,,,IS THERE A GOOD GLUE OUT THERE that will do the same thing as the HOTLINE FUSERS GLUE, that i can buy by the 10lb bag, that wont leave any residue on the glass, when make a PATE DE VERRE PASTE,,, thanks, rodney
			 
			
					
				pate de verre glue
				Posted: Mon May 19, 2003 10:05 pm
				by Carol Craiglow
				Hi Rodney....Here's another souce:
http://www.fusionheadquarters.com/Pages ... Verre.html
I haven't used it, but a friend of mine has and says it works well.
Carol
 
			 
			
					
				
				Posted: Tue May 20, 2003 7:32 am
				by Colin & Helen
				The last time I purchased fusers glue it ended up with a green fungus happily growing in the jar.. now I have gone back to using Ploycell wall paper paste ..with out any problems...Colin